Remove all loose, cracked, hardened and/or deteriorated caulking presently installed at all metal to stucco, and wood to stucco perimeter joints, around windows, door frames, decorative stucco bands and any other trim.
After removing old caulking material, the joints are then cleaned and sealed.
To insure a waterproof seal, a complete and continuous new bead of Manufacturer's specified caulk will be applied over the joint in a smooth seamless manner to insure proper adhesion and appearance.
All hairline cracks will be detailed and patched with a Manufacturer specified elastomeric textured patching compound. The cracks will be scraped on the center, cleaned, primed and filled in the middle overlapping at approximately 2 inches on both sides. Larger structural cracks will be injected with a urethane sealant and then finished with elastomeric patch to match existing texture as close as possible.
|
|
|
|
|
 |
| |
 |
|
|
|
|